Sandvik 446-4C54 Billet
Subcategory: Stainless Steel; Metal; Ferritic
Close Analogs: ASTM 446; UNS S44600; EN 1.4749
Material Notes: Sandvik 4C54 is a ferritic, heat resisting, stainless chromium steel, characterised by: extremely good resistance to reducing sulphurous gases
very good resistance to oxidation in airgood resistance to oil-ash corrosiongood resistance to molten copper, lead and tinThis steel can be used at temperatures up to 1100°C (2010°F). However, allowance should be made for the low creep strength at the highest temperatures in order to avoid distortion due to the mass of the steel. Information provided by Sandvik
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Rupture Strength
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|