Sandvik F45-10R19 Billet
Subcategory: Stainless Steel; Nickel Alloy; Metal; Austenitic
Close Analogs: UNS S30815; EN 1.4835
Material Notes: Sandvik 10R19 is an austenitic chromium-nickel steel alloyed with nitrogen and rare earth metals. The grade is characterised by: high creep strength very good resistance to isothermal and, above all, cyclic oxidationvery good resistance to combustion gasesgood structural stability at high temperatures good weldabilitythe grade can be used at temperatures up to about 1150°C (2100°F). Information provided by Sandvik
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|