Sandvik SAF 2507 Billet
Subcategory: Stainless Steel; Metal; Duplex
Close Analogs: UNS S32750; EN 1.4410
Material Notes: Sandvik SAF 2507 is a high alloy duplex (austenitic-ferritic) stainless steel for service in highly corrosive conditions. It is characterised by: excellent resistance to stress corrosion cracking in chloride bearing environments excellent resistance to pitting and crevice corrosion high resistance to general corrosion very high mechanical strengthphysical properties that offer design advantageshigh resistance to erosion corrosion and corrosion fatigue good weldabilityInformation provided by Sandvik
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- CTE, linear 100°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|