Sandvik Sanicro 41 Billet
Subcategory: Alloy Steel; Metal
Close Analogs: UNS N08825; EN 2.4858
Material Notes: Sandvik Sanicro 41, commonly known as Alloy 825, is an austenitic corrosion-resistant Ni-Fe-Cr alloy with the following properties: Excellent resistance to stress corrosion cracking in chloride and sour (H2S/Cl- ) environments. Excellent resistance to attack by acidic media such as sulphuric acid and phoshoric acid Better resistance to pitting and crevice corrosion compared to steels of the AISI 316 typeGood weldabilityInformation provided by Sandvik
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|