Sandvik Sanicro 70 Billet
Subcategory: Alloy Steel; Metal
Close Analogs: UNS N06600; EN 2.4816
Material Notes: Sandvik Sanicro 70, commonly known as Alloy 600, is an austenitic nickel-chromium-iron alloy, characterised by very good resistance to carburisation and nitrogen absorption and good structural stability at high temperatures. It has also good resistance to stress corrosion cracking.Information provided by Sandvik
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|