Sandvik SANMAC 4571 Billet
Subcategory: Alloy Steel; Metal
Close Analogs: ASTM 316Ti; UNS S31635; EN 1.4571
Material Notes: Sanmac 4571, 1.4571/316Ti, is a titanium stabilized, molybdenium-alloyed austenitic chrome-nickel steel with improved machinability.Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|