Sandvik 253 MA Plate, Sheet and Coil
Subcategory: Nickel Alloy; Alloy Steel; Metal
Close Analogs: UNS S30815; EN 1.4835
Material Notes: Sandvik 253 MA is an austenitic chromium-nickel steel alloyed with nitrogen and rare earth metals. The grade is characterised by: high creep strength very good resistance to isothermal and, above all, cyclic oxidationgood structural stability at high temperaturesgood weldability the grade can be used at temperatures up to about 1150°C (2100°F).Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Creep Strength
- Rupture Strength
- Modulus of Elasticity
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|