Sandvik 304 Plate, Sheet and Coil
Subcategory: Nickel Alloy; Alloy Steel; Metal
Close Analogs: ASTM 304; UNS S30400; EN 1.4301
Material Notes: Grade 304 is an austenitic chromium-nickel steel.Information provided by Sandvik