Sandvik SAF 2304 Plate, Sheet and Coil
Subcategory: Stainless Steel; Alloy Steel; Low Carbon Steel; Metal; Duplex
Close Analogs: UNS S32304; EN 1.4362
Material Notes: Duplex stainless steel, UNS S32304Sandvik SAF 2304TM is a duplex stainless steel (austenitic-ferritic) with a low carbon content. The material is characterised by the following properties: very good resistance to stress corrosion cracking.good resistance to general corrosion an pitting. high strength - approximately twice as high proof strength as austenitic stainless steels.physical properties that offer design advantages. ease of fabrication and good toughness.good weldability
Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Modulus of Elasticity
- Charpy Impact
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|