Sandvik 11RM20 Precision Wire
Subcategory: Stainless Steel; Alloy Steel; Metal; Austenitic
Close Analogs: ASTM 201; EN 1.4371
Material Notes: Sandvik 11RM20 is an austenitic stainless steel delivered in flat rolled condition and used primarily for expander rings on automotive engine pistons. The grade can also be delivered as round drawn wire.Information provided by Sandvik
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Modulus of Elasticity
- Shear Modulus
|
|
|
|
| Property Data |