Sandvik Bioline 1RK91 Precision Wire
Subcategory: Stainless Steel; Precipitation Hardening Stainless; Metal; Ferritic
Material Notes: Sandvik Bioline 1RK91 (a Sandvik NanoflexTM material) is a precipitation hardening stainless steel grade specifically designed for applications requiring high strength combined with good ductility in the final product and high formability in the as-delivered condition. The strength is increased after ageing of the final product.The characteristics in general can be said to be a combination of properties of ordinary austenitic stainless and low alloyed ferritic steels. This means that properties such as elastic modulus, mechanical properties and thermal expansion are comparable to ferritic steels (such as low alloyed carbon steels or chromium steels) while properties such as corrosion resistance is more comparable to austenitic stainless steels. excellent mechanical properties, very high tensile strength and hardness levels can be achieved corrosion resistance comparable to AISI 304L or AISI 316L depending on condition retained mechanical properties at temperatures up to at least 400oC
good weldabilityInformation provided by Sandvik
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Modulus of Elasticity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|