Sandvik 2C48 Seamless tube and pipe
Subcategory: Stainless Steel; Metal; Ferritic
Close Analogs: ASTM 446-2; UNS S44600
Material Notes: Sandvik 2C48 is a ferritic, heat resisting, stainless chromium steel, characterised by: good resistance to reducing sulphurous gasesvery good resistance to oxidation in air good resistance to oil-ash corrosionresistance to molten copper, lead and tinThis steel can be used at temperatures up to 1075 °C (1970 °F). However, allowance should be made for the low creep strength at the highest temperatures in order to avoid distortion due to the mass of the steel. Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|