Sandvik 2RE69 Seamless tube and pipe
Subcategory: Stainless Steel; Metal; Austenitic; Ferritic
Close Analogs: UNS S31050; EN 1.4466
Material Notes: Sandvik 2RE69 is a fully austenitic stainless steel with extra low carbon and impurity contents. The grade is primarily developed in order to cope with the severe corrosive conditions existing in the urea industry. The characteristics of Sandvik 2RE69 are: Excellent resistance to corrosion in ammonium carbamate and nitric acid Excellent resistance to intergranular corrosionHigh resistance to pitting and crevice corrosion Good weldabilityInformation provided by Sandvik
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Modulus of Elasticity
- Magnetic Permeability
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|