Sandvik 2RK65 Seamless tube and pipe
Subcategory: Stainless Steel; Nickel Alloy; Metal; Austenitic
Close Analogs: UNS N08904; EN 1.4539
Material Notes: Sandvik 2RK65 is an austenitic stainless ELC steel intended for use under severe corrosion conditions within the process industry. The material is characterised by the following properties: very good resistance to attacks in acidic environments, e.g. sulphuric, phosphoric and acetic acid very good resistance to pitting in neutral chloride-bearing solutionsmuch better resistance to crevice corrosion than steels of the AISI 304 and AISI 316 type very good resistance to stress corrosion crackinggood weldabilityInformation provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|