Sandvik 353 MA Seamless tube and pipe
Subcategory: Nickel Alloy; Metal
Close Analogs: UNS S35315; EN 1.4854
Material Notes: Sandvik 353 MA is an austenitic chromium-nickel steel alloyed with nitrogen and rare earth metals. The grade is characterised by: high creep strength very good resistance to isothermal and cyclic oxidationvery good resistance to combustion gasesvery good resistance to carburisationgood resistance to nitriding gasesgood structural stability at high temperaturesgood weldabilitythe grade can be used at temperatures up to about 1175°C (2150°F).Sandvik manufactures 353 MA under licence from Avesta Sheffield AB. Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Creep Strength
- Rupture Strength
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|