Sandvik 3R12 Seamless tube and pipe
Subcategory: Nickel Alloy; Low Carbon Steel; Metal; Austenitic
Close Analogs: ASTM 304, 304L; UNS S30400, S30403; EN 1.4301, 1.4306
Material Notes: Sandvik 3R12 is an austenitic chromium-nickel steel with a low carbon content.Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Rupture Strength
- Modulus of Elasticity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|