Sandvik 3R64 Seamless tube and pipe
Subcategory: Stainless Steel; Metal; Austenitic
Close Analogs: ASTM 317L; UNS S31703
Material Notes: Austenitic high molybdenum stainless steel, ASTM TP 317LSandvik 3R64 is an austenitic stainless steel with a high molybdenum content. Significant properties are improved general and pitting corrosion resistance in comparison with AISI 316L. Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Modulus of Elasticity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |