Sandvik 3R65 Seamless tube and pipe
Subcategory: Low Carbon Steel; Metal; Austenitic
Close Analogs: ASTM 316, 316L; UNS S31603, S31600; EN 1.4404, 1.4401
Material Notes: Sandvik 3R65 is a molybdenum-alloyed austenitic chromium-nickel steel with a low carbon content.Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Modulus of Elasticity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|