Sandvik 5R75 Seamless tube and pipe
Subcategory: Stainless Steel; Nickel Alloy; Metal; Austenitic
Close Analogs: ASTM 316Ti; UNS S31635; EN 1.4571
Material Notes: Austenitic stainless steel, AISI type 316TiSandvik 5R75 is an austenitic, titanium-stabilised stainless chromium–nickel–molybdenum steel. Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Modulus of Elasticity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.