Sandvik 7RE10 Seamless tube and pipe
Subcategory: Stainless Steel; Nickel Alloy; Metal; Austenitic
Close Analogs: ASTM 310S, 310H; USN S31008, S31009; EN 1.4845
Material Notes: Sandvik 7RE10 is an austenitic, stainless chromium-nickel steel of the 25/20 type, suitable for high temperature applications. The grade is characterised by: Good resistance to carburization, sulphidation and oxidation combined with moderate creep strength and structural stability. A maximum service temperature in air of 1100°C (2010°F).Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Rupture Strength
- Modulus of Elasticity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|