Sandvik Sanicro 30 Seamless tube and pipe
Subcategory: Nickel Alloy; Low Carbon Steel; Metal; Austenitic
Close Analogs: UNS N08800; EN 1.4558
Material Notes: Nickel-iron-chromium alloy, Low carbon version, UNS N08800Sandvik Sanicro 30 is a low-carbon version of the austenitic nickel-iron-chromium alloy. It is used for steam generator tubing in nuclear stations (PWR) and other heat exchangers for temperature up to about 550°C (1020 °F) where good resistance to stress corrosion cracking and intergranular corrosion is required. Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|