Sandvik Sanicro 41 Seamless tube and pipe
Subcategory: Nickel Alloy; Metal
Close Analogs: ASTM 825; UNS N08825; EN 2.4858
Material Notes: Sandvik Sanicro 41 is an austenitic, corrosion resistant Ni-Fe-Cr alloy. The grade is characterized with the following properties:excellent resistance to stress corosion cracking in chloride and sour (H2S/Cl- ) environments excellent resistance to attack by acidic media such as sulphuric acid better resistance to pitting and crevice corrosion than steels of the AISI 316 typegood weldabilityInformation provided by Sandvik
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|