Sandvik Sanicro 31HT Seamless tube and pipe
Subcategory: Nickel Alloy; Metal
Close Analogs: UNS N08811, N08810; EN 1.4959
Material Notes: Sandvik Sanicro 31HT is an austenitic nickel-iron-chromium alloy characterised by: high creep strengthvery good resistance to oxidation good resistance to combustion gasesvery good resistance to carburizationgood resistance to nitrogen absorptiongood structural stability at high temperatures good weldabilitySandvik Sanicro 31HT can be used at temperatures up to about 1100°C (2010°F). In order to have the best ductility, it should be used above 700 °C (1290 °F). We can also supply a modified version of Sandvik Sanicro 31HT for use in the temperature range between about 550 and 700°C (1020-1290°F). The chemical composition and heat treatment of this version have been adapted for the highest possible creep ductility. Further information on properties is available on request. Sandvik Sanicro 31HT is not generally used under wet corrosive conditions. For this type of environment, we recommend Sandvik Sanicro 30, which is specially adapted for wet corrosive conditions up to about 550°C (1020°F). For further details, see the Sandvik Sanicro 30 datasheet on our website (www.smt.sandvik.com) or in printed form (S-1890-ENG). Information provided by Sandvik
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Rupture Strength
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|