Sandvik Kanthal SW 200 Spray Wire
Subcategory: Special-Purpose Steel; Metal; Austenitic
Material Notes: KANTHAL SW 200 is an austenitic NiCr alloy developed for use in Arc and Flame Spray systems. The wire produces dense, well bonding coatings resistant to high temperature oxidation. Typical applications are as protective coatings against corrosive gases, protection against scaling of conventional low alloy steels, build up coatings for dimensional restoration.Information provided by Sandvik
| Available Properties |
- Density
- Porosity
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Electrical Resistivity
- Melting Point
- Deposition efficency, %
- Oxides, %
- Surface Roughness, microns
|
|
|
|
| Property Data |