Sandvik SAF 2205 Spring Wire
Subcategory: Stainless Steel; ASTM Steel; Special-Purpose Steel; Metal; Duplex
Close Analogs: UNS S31803; EN 1.4462
Material Notes: Sandvik SAF 2205 is a duplex stainless steel (austenitic-ferritic). It is characterised by:high resistance to stress corrosion cracking in chloride-bearing environmentshigh resistance to stress corrosion cracking in environments containing hydrogen sulphidehigh resistance to general corrosion, pitting, and crevice corrosionhigh resistance to erosion corrosion and corrosion fatiguephysical properties that offer design advantagesService temperature: -100 to 300°C (-150 to 570°F) Information provided by Sandvik
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Modulus of Elasticity
- Shear Modulus
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|