Sandvik Santex Spring Wire
Subcategory: Stainless Steel; Special-Purpose Steel; Metal
Material Notes: Sandvik Santex is a high quality stainless steel grade optimal for applications with a high number of cycles where the springs have to retain their mechanical properties under a long period of time. The steel grade has excellent spring properties combined with a high fatigue resistance and a low relaxation rate.Information provided by Sandvik
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Modulus of Elasticity
- Shear Modulus
- Specific Heat Capacity
|
|
|
|