Sandvik 13RM19 Strip Steel
Subcategory: Stainless Steel; Special-Purpose Steel; Metal
Material Notes: Sandvik 13RM19 is a stainless spring steel combining high mechanical strength with a non-magnetic structure. This combination of properties has previously been found mainly in expensive Co-Ni-base or Cu-Be-alloys. The corrosion resistance is comparable to that of ASTM 301. Sandvik 13RM19 is characterised by: non-magnetic structure in all conditionshigh mechanical strength in the cold rolled condition. The strength can be further increased without any effect on the non-magnetic structure by tempering.high elastic limit and energy storing capacity in the cold rolled and tempered condition Sandvik 13RM19 also possesses good fatigue properties and excellent ductility, which makes it a most suitable choice for springs and other high strength applications where ferromagnetic materials cannot be used. Service temperature: up to 250°C (480°F) Information provided by Sandvik
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Modulus of Elasticity
- Fatigue Strength
- Electrical Resistivity
- CTE, linear 100°C
- CTE, linear 250°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|