Sandvik 20C Strip Steel
Subcategory: ASTM Steel; Special-Purpose Steel; Metal
Close Analogs: ASTM 1095; EN 1.1274
Material Notes: Sandvik 15LM and 20C are characterised by good properties in respect of: Fatigue strength and wear resistanceHardness combined with ductility Dimensional tolerancesSurface and edge finishesShapeThe materials also have good blanking and forming properties with retaining shape of the parts after the blanking operation. Information provided by Sandvik
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- CTE, linear 100°C
- CTE, linear 250°C
- Thermal Conductivity
|
|
|
|