Nistelle® alloy C-4C
Subcategory: Superalloy; Nickel Base
Key Words: Deloro Stellite Inc.
Material Notes: Nickel content as balance. Comparable to Tribaloy Alloy 745. Data provided by the manufacturer, Deloro Stellite Inc.