Stellite® alloy STAR J-Metal PM, P/M, tested at RT

 

Subcategory: Superalloy; Cobalt Base

Key Words: Deloro Stellite Inc.

Material Notes:
Cobalt content as balance.

Applications: Vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, wear pads, pins, balls, hardfaces when crack free deposits are not required.

Corrosion: Corrosion resistance similar to Stellite alloy 3, but inferior to Stellite alloy 6. Excellent oxidation resistance at low temperatures, but not recommended for reducing environments. Corrosion will vary depending on concentration, temperature, stress, and type of contaminants so exposure tests are recommended.

Machinability: Stress relieve before and during machining by holding at 900°C (1650°F) for four hours and slow cool.

Wear: High tungsten content results in excellent hot hardness and low stress abrasion resistance superior to Stellite alloy 3. Wear resistance is similar to Stellite alloy 3 and is non-galling when mated with other Stellite alloys.

Data provided by the manufacturer, Deloro Stellite Inc.

Available Properties
  • Density
  • Hardness, Rockwell C
  • Tensile Strength, Ultimate
  • Elongation at Break
  • Modulus of Elasticity
  • Magnetic Permeability
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。