Stoody® 4 Cobalt-Base Cast Alloy
Subcategory: Superalloy; Nonferrous Metal; Cobalt Base
Key Words: Deloro Stellite Inc.
Material Notes: Cobalt content above calculated as balance. Stoody® 4 is a cobalt-base alloy with excellent high temperature strength and generally better corrosion resistance than Alloys 1 and 6. This centrifugally cast alloy derives is good high temperature strength from the high Tungsten to Carbon ratio which allows a large percentage of Tungsten to remain in solid solution. Recommended for dies, in hot pressing or extrusion of Copper base and Aluminum Alloys, high temperature steam turbine components and other applications where high temperature wear/abrasion, corrosion/erosion is present. This alloy is also particularly suited in applications involving Manganese Dioxide, Carbon particles and Ammonium Zinc Chlorides such as in dry battery mixes. Information provided by Deloro Stellite Inc.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|