Stoody® 5 Cobalt-Base Cast Alloy
Subcategory: Superalloy; Nonferrous Metal; Cobalt Base
Key Words: Deloro Stellite Inc.
Material Notes: Cobalt content above calculated as balance. Stoody® 5 is a high carbon, chromium, tungsten, iron, cobalt-base centrifugally cast alloy. This alloy is basically a modification of Stoody 1 where good wear properties are required and greater resistance to impact and thermal shock is required. Recommended for steel mill guide roll applications. Information provided by Deloro Stellite Inc.
|
|
|