Stoody® 6 Cobalt-Base Alloy

 

Subcategory: Superalloy; Nonferrous Metal; Cobalt Base

Key Words: MIL-C-15345G, Alloy 20, and MIL-C-24248; Deloro Stellite Inc.

Material Notes:
Cobalt content above calculated as balance.

Stoody® 6 is a cobalt-base alloy with high abrasion, corrosion, and elevated temperature wear resistance. Its wear resistance is in a class ordinarily associated with hard metals. Chief differences between Stoody 6 and Stoody 1 is a lower proporiton of tungsten and carbon. Abrasion resistance is somewhat decreaed, while impact strength is increased.

This alloy is recommended for applications involving restance to room and high temperature abrasive action, galling in metal to metal wear, and a moderate degree of impact, thermal shock or stress loading. Typical uses of Stoody 6 are bearings, for pumps, saran extruder cylinder liners, pivot bearings, and forming dies. Stoody 6 with minor modifications can be manufactured to coform to Military Specification MIL-C-15345G, Alloy 20, and MIL-C-24248 (ships), Compostion I.

Information provided by Deloro Stellite Inc.

Available Properties
  • Hardness, Rockwell C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。