Stellite® alloy 6K, 1.6 mm thick sheet, tested at 1093°C
Subcategory: Superalloy; Cobalt Base
Key Words: Deloro Stellite Inc.
Material Notes: Cobalt content as balance. 13.3 mm^3 volume loss--abrasive wear data. Applications include agitators, augers, ball mills, banbury mills, cams, crusher bearings, dryers, dry presses, dump cars, fans, filters, food machinery, galvanizing roll necks, grinder ring bearings, marine equipment, mixing equipment, pulleys, pump seals, pump shafts, rotary kilns, scraper rolls, screw conveyors, spindles, stuffing boxes, thickeners, tile presses, wear bars. Data provided by the manufacturer, Deloro Stellite Inc.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Magnetic Permeability
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|