Swiss Steel International THYRODUR® 2990 Cold Work Steel
Subcategory: Tool Steel; Cold Work Steel; Metal
Close Analogs: Iron content calculated as remainder
Key Words: 1.299
Material Notes: Cold Work Steels, because of their typical properties - high surface hardness, good toughness and compressive strength, high wear resistance - find use as cutting and pressing tools, cavity moulds and knives, hobbing and drawing tools, cavity sinking punches, flat and circular thread-rolling dies and much more.New developed ledeburtic cold work tool steel with high hardness, good toughness and high resistance to tempering combined with high wear resistance Applications - Cutting and stamping tools
- Fine cutting tools
- Thread rolling dies
- Circular-shear blades
- Cold pilger mandrels
- Pressure pads and plastic molds
- Cold extrusion tools and deep drawing tools
- Wood cutting knives
- Cold rolls
| Available Properties |
- Hardness, Brinell
- Hardness, Rockwell C
- CTE, linear 20°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Annealing Temperature
- Cooling
- Hardening from: °C
- Quenching
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|