Swiss Steel International Brake Die 2312 Cold Work Steel
Subcategory: Cold Work Steel; Metal
Close Analogs: Iron content calculated as remainder
Material Notes: Cold Work Steels, because of their typical properties - high surface hardness, good toughness and compressive strength, high wear resistance - find use as cutting and pressing tools, cavity moulds and knives, hobbing and drawing tools, cavity sinking punches, flat and circular thread-rolling dies and much more.Brake Die is an electric arc melted vacuum degassed alloy steel supplied in the prehardened condition to 32 HRC (300HB) hardness. Its machinability is superior to that of AISI grades 4140 and 4150. Brake Dieexhibits an excellent combination of strength, toughness and wear resistance. Applications - Press brake dies
- Pressure pads
- Holders
- Forming Dies
- Machinery Components
| Available Properties |
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- CTE, linear 20°C
- Thermal Conductivity
- Cooling
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|