Swiss Steel International THYROTHERM® 2344 EFS Hot Work Steel
Subcategory: Tool Steel; Hot Work Steel; Metal
Close Analogs: Iron content calculated as remainder
Key Words: 1.2344
Material Notes: The properties of Hot Work Steels are matched specifically to high-temperature applications. Typical fields of use for hot work steels include: die casting, extrusion, die forging, glass processing, and tube and pipe manufacture.High hot-wear resistance, high hot tensile strength and toughness. Good thermal conductivity and insusceptibility to hot cracking. Can be water cooled to a limited extent. Applications - Pressure casting dies and metal extrusion tools for processing light materials
- Forging Dies
- Molds
- Screws and barrels for plastic processing
- Shrink rings
- Hot-shear blades
| Available Properties |
- Hardness, Brinell
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- CTE, linear 20°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Annealing Temperature
- Cooling
- Hardening from: °C
- Quenching
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|