Swiss Steel International THYROTHERM® 2344 Magnum Hot Work Steel
Subcategory: Tool Steel; Hot Work Steel; Metal
Close Analogs: Iron content calculated as remainder
Key Words: AISI H13 Premium
Material Notes: The properties of Hot Work Steels are matched specifically to high-temperature applications. Typical fields of use for hot work steels include: die casting, extrusion, die forging, glass processing, and tube and pipe manufacture.Thyrotherm 2344 Magnum is an electro slag remelted hot work tool steel, designed to meet all premium H13 specifications. The increased toughness of this material was developed to meet the most stringent die casting applications. Thyrotherm 2344 Magnum differs from Thyrotherm 2344 SUPRA by using specially selected input materials, controlled forging, and special thermal procedures.
| Available Properties |
- Hardness, Brinell
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- CTE, linear 20°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Annealing Temperature
- Cooling
- Hardening from: °C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|