Swiss Steel International THYROTHERM® 2885 EFS Hot Work Steel
Subcategory: Tool Steel; Hot Work Steel; Metal
Close Analogs: Iron content calculated as remainder
Key Words: 1.2885, AISI H 10 A
Material Notes: The properties of Hot Work Steels are matched specifically to high-temperature applications. Typical fields of use for hot work steels include: die casting, extrusion, die forging, glass processing, and tube and pipe manufacture.Cr-Mo-Co-alloyed hot-work tool steel with high resistance to thermal fatigue and high-temperature strength. Applications - Diecasting tools
- Hot-pressing tools
- Extrusion tools
- Mainly for heavy metals
| Available Properties |
- Hardness, Brinell
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- CTE, linear 20°C
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
- Annealing Temperature
- Cooling
- Hardening from: °C
- Quenching
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|