Nickel Alloy 59, UNS N06059
Subcategory: Superalloy; Nickel Alloy; Nonferrous Metal; Nickel Base
Close Analogs: Nickel content calculated as remainder.
Key Words: Nicrofer® 59
Material Notes: This alloy is noted for its resistance to a wide range of corrosive environments, both oxidizing and reducing. This alloy was developed by ThyssenKrupp VDM.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Impact
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Solution Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|