TIMETAL® 1100 Titanium Alloy (Ti-6Al-2.7Sn-4Zr-0.4Mo-0.45Si)
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Near Alpha Titanium Alloy
Material Notes: Titanium content above is calculated as the remainder and may not reflect the actual range. Features: A near alpha, high temperature creep resistant alloy developed for elevated temperature use in the range of 600°C that offers the highest combination of strength, creep resistance, fracture toughness and fatigue crack growth resistance. Data provided by TIMET.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Fatigue Strength
- Bend Radius, Minimum
- Maximum Service Temperature, Air
- Beta Transus
|
|
|
|