TIMETAL® Code 12 Titanium Alloy (ASTM Grade 12)
Subcategory: Titanium Alloy; Nonferrous Metal; Unalloyed/Modified Titanium
Key Words: UNS R53400
Material Notes: Features: Highly weldable, near-alpha alloy, exhibiting improved strength and temperature capability over CP combined with superior crevice corrosion resistance and excellent resistance under oxidizing to mildly reducing conditions especially chlorides. Data provided by TIMET.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Fatigue Strength
- Bend Radius, Minimum
- Beta Transus
|
|
|
|