TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al), Anneal Strip/Sheet
Subcategory: Titanium Alloy; Nonferrous Metal; Beta Titanium Alloy
Material Notes: Titanium content above is calculated as the remainder and may not reflect the actual range. High-Strength, Cold Formable Strip Alloy Industry Specifications: USA Aerospace: AMS 4914A. Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vessels and other fabricated sheet metal structures up to 300°C. Typical heat treatment for this alloy: Solution Treatment: 790°C for 3-20 min, air cool. Age Treatment: 480-620°C for 4-16 hrs. Data provided by TIMET.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Bend Radius, Minimum
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Beta Transus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|