TIMETAL® 17 Titanium Alloy (Ti-5Al-2Sn-4Mo-2Zr-6Mo); Aged Billet/Bar
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy
Key Words: UNS R52252
Material Notes: Titanium content above is calculated as the remainder and may not reflect the actual range. Features: High strength, deep hardenable forging alloy primarily for jet engines. Allows heat treatment to a variety of strength levels in sections up to 6 inches. Offers good ductility and toughness, as well as good low cycle and high cycle fatigue properties. Data provided by TIMET.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Fatigue Strength
- Beta Transus
|
|
|
|