TIMETAL® 21S Titanium Alloy (Ti-15Mo-3Nb-3Al-0.2Si, ASTM Grade 21); Aged at 593°C

 

Subcategory: Titanium Alloy; Nonferrous Metal; Beta Titanium Alloy

Key Words: Beta 21S; UNS R58210

Material Notes:
Titanium content above is calculated as the remainder and may not reflect the actual range.

High-Strength, Oxidation Resistant Strip Alloy

Features: Offers the good cold formability and weldability of a beta strip alloy, but with greatly improved oxidation resistance and creep strength. Aerospace applications include engine exhaust plug and nozzle assemblies. The alloy's resistance to aircraft hydraulic fluids, such as Skydrol, is excellent at all temperatures. It is well suited for metal matrix composites because it can be economically rolled to foil, is compatible with most fibers, and is sufficiently stable up to 816°C.

Typical heat treatment for this alloy: Solution treatment: 816-843°C for 3-30 min, air cool. Age treatment: 510-679°C for 8-16 hrs.

Data provided by TIMET.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Beta Transus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。