TIMETAL® 3-2.5 Titanium Alloy (Ti-3Al-2.5V; ASTM Grade 9) Annealed

 

Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Near Alpha Titanium Alloy

Key Words: Titanium 3-2.5; UNS R56320

Material Notes:
Titanium content above is calculated as the remainder and may not reflect the actual range.

Cold Workable Medium Strength Alloy. UTS, TYS, Elongation, R.A. and bend radius data below are specific to annealed material; other specific condition entries are also available in MatWeb.

Features: Cold formable and weldable, this alloy is used primarily for honeycomb foil and hydraulic tubing applications. Industrial applications such as pressure vessels and piping also utilize this alloy. Available with palladium stabilization to enhance corrosion resistance. The alloy is cold formable and easily welded, such like the commercially pure grades of titanium. Yet the alloys offer nearly double the strength over TIMETAL 50A. It is ASME Boiler and Pressure Vessel code approved. It offers the highest structural efficiency of any of the common engineering metals approved by ASME. The alloy is available in all common product forms including billet, bar, plate, sheet, strip, tubing and pipe. It is nonmagnetic.

Typical heat treatment for this alloy: Stress Relief: 316-649°C for .5-3 hrs, air cool. Anneal: 649-760°C for 1-3 hrs, air cool. Solution treat: 871-927°C for .25-1 hrs, water quench. Aging: 482-538°C for 2-8 hrs, air cool.

Data provided by TIMET.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Bend Radius, Minimum
  • Electrical Resistivity
  • CTE, linear 20°C
  • Thermal Conductivity
  • Melting Point
  • Liquidus
  • Beta Transus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。