TIMETAL® 50A CP Titanium (ASTM Grade 2)

 

Subcategory: Titanium Alloy; Nonferrous Metal; Unalloyed/Modified Titanium

Key Words: UNS R50400

Material Notes:
Titanium content above is calculated as the remainder and may not reflect the actual range.

Commercially Pure Titanium.

Industry Specifications: USA Aerospace: AMS 4902, 4941. Germany Engineering: 3.7035. Germany Aerospace: 3.7034. France: T-40. UK Aerospace Specifications BS TA. 2, 3, 4, 5.

Features: The mechanical properties of CP titanium are influenced by small additions of oxygen and iron. By careful control of these additions, the various grades of commercially pure titanium are produced to give properties suited to different applications. TIMETAL 50A is equivalent to ASTM Grade 2. It is the "workhorse" for industrial applications, having a guaranteed minimum 0.2% yield strength and good ductility and formability. It is used extensively for sea water piping, reactor vessels and heat exchangers throughout the CPI, Petrochemical, Oil and Gas and Naval/Marine markets. This alloy is also ASME approved, has good impact properties at low temperatures, and has excellent resistance to erosion and corrosion by seawater and marine atmospheres. It can be easily welded, machined, cold worked, hot worked, and cast. It is nonmagnetic.

Typical heat treatment for this alloy: Anneal at 700°C for 1 hour and air cool. Stress Relieve at 500°C for 30 mins and air cool.

Data provided by TIMET.

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Modulus of Elasticity
  • Fatigue Strength
  • Bend Radius, Minimum
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Beta Transus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。