TIMETAL® 5111 Titanium Alloy (Ti-5Al-1Sn-1Zr-1V-0.8Mo; ASTM Grade 32)
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Near Alpha Titanium Alloy
Material Notes: Titanium content above is calculated as the remainder and may not reflect the actual range. High Toughness, Heavy Section Weldable Alloy Features: A near alpha alloy with excellent weldability, seawater stress corrosion cracking resistance and high dynamic toughness. It is ideally suited for applications in marine environments where toughness and corrosion resistance are essential. The alloy has been produced on a commercial scale. It was developed jointly with the Navy, and has been selected as the material of choice for a submarine application. Data provided by TIMET.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Bend Radius, Minimum
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
- Beta Transus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|