TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Alpha-Beta Forged, RA
Subcategory: Titanium Alloy; Nonferrous Metal; Beta Titanium Alloy
Material Notes: Titanium content above is calculated as the remainder and may not reflect the actual range. Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Alpha-Beta Forged, RA material. Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but with significantly higher stiffness (elastic modulus). Due to the use of iron as the beta stabilizer, the alloy has lower formulation costs than TIMETAL 6-4. The combination of reasonable cost and excellent mechanical properties make TIMETAL 62S a practical substitute for many engineering materials. Typical heat treatment for this alloy: Mill Anneal at 760°C for 1-2 hrs, air cool Data provided by TIMET.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Modulus of Elasticity
- Fracture Toughness
- Bend Radius, Minimum
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Beta Transus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|