TIMETAL® 6-4-.1Ru Titanium Alloy (Ti-6Al-4V-0.1Ru; ASTM Grade 29)
Subcategory: Titanium Alloy; Nonferrous Metal; Alpha/Beta Titanium Alloy
Key Words: Titanium 6-4
Material Notes: Titanium content above is calculated as the remainder and may not reflect the actual range. Medium To High Strength General-Purpose Alloy. Property data below are typical of Timet® 6-4 ELI (without Ru). The 0.1 Ru ELI variant is used for enhanced corrosion resistance. Data provided by TIMET.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Bend Radius, Minimum
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Melting Point
- Liquidus
- Maximum Service Temperature, Air
- Beta Transus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|